Industrial Systems and Manufacturing Instructor
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Aluminum Etc.: You can cut aluminum on a CNC plasma system
How a welder/fabricator can get the best results cutting aluminum with CNC plasma
- By Gina Cutts
- UPDATED March 6, 2024
- March 5, 2024
People still tell me confidently that you can’t cut aluminum on a CNC plasma cutting table—even as they watch me cut aluminum with a CNC table right in front of them.
Sometimes old information or a lack of awareness of the advancements that have been made in plasma cutting technology prevent CNC enthusiasts from making projects out of aluminum. With aluminum being both corrosion resistant and so much lighter than steel, they are really missing out!
Modern plasma cutting systems are more capable and adaptable to different materials than older models. So, yes, you can use a plasma cutting table to cut aluminum sheets.
Confusion about aluminum and plasma tables might occur because people do not understand three key points:
- Material conductivity - Plasma cutting relies on the electrical conductivity of the material being cut. Aluminum is a highly conductive material, making it suitable for plasma cutting.
- Material thickness - Plasma cutting is effective for a variety of material thicknesses, but the thickness and the power of the plasma cutter need to be matched appropriately. Frustration can occur if someone attempts to cut aluminum that is too thick for their plasma cutting setup.
- Settings and gas selection - The settings and gas used in plasma cutting can impact cut quality. When cutting aluminum, specific adjustments in power settings and gas selection are necessary for optimal results. If these adjustments are not made, it may lead to poor cut quality and misconceptions about the process.
Some considerations and adjustments that need to be made when cutting aluminum with a plasma cutter include:
- Power settings - Aluminum has different thermal conductivity compared to steel, so you may need to adjust the power settings on your plasma cutter. Consult the manufacturer's recommendations for cutting aluminum with your specific machine.
- Gas selection - When cutting aluminum, it's common to use nitrogen or a nitrogen/argon mix as the plasma gas instead of regular compressed air. This helps prevent oxide formation on the cut edges and produces a cleaner cut. Make sure you don’t overlook this critical factor.
- Cutting speed - Aluminum generally requires a slower cutting speed than steel. Adjust the cutting speed according to the thickness of the aluminum sheet you are working with.
- Consumables - Make sure to use the appropriate consumables for cutting aluminum. This may include a specific type of nozzle and electrode designed for aluminum cutting.
- Cleanliness - Ensure the aluminum sheets are clean and free of any contaminants or coatings that could affect the cutting process.
Always refer to the manufacturer's guidelines and recommendations for cutting aluminum with your specific plasma cutting table. Additionally, it's a good idea to conduct test cuts on scrap material to fine-tune your settings before you begin your project. It's essential for individuals using a CNC plasma cutting system to be well informed about the specific requirements and adjustments needed for cutting aluminum.
I would love to see your aluminum CNC projects! You can email me pictures at ginac@bigbend.edu.
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscriptionAbout the Author
About the Publication
- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
How welders can stay safe during grinding
Connecticut students compete in Maritime Welding Competition
Three ESAB welding machines win Red Dot Awards for product design
- Industry Events
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,