Editor
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Cobot helps build capacity at Skyvington Manufacturing
Store fixture supplier sees benefits of investments in welding tables, flexible automation
- By Robert Colman
- Updated January 11, 2024
- January 9, 2024
- Article
- Automation and Robotics
Editor’s Note: This feature originally appeared in the September 2023 issue of Canadian Fabricating & Welding.
When Skyvington Manufacturing Inc. (SMI) wanted to add capacity to its welding shop, the management team knew that it would require an investment either in more skilled welders or automation. Although automation was the obvious choice in this era of ever-decreasing lead times, the company wanted to find the right fit for the shop’s product mix.
Company History
Founded by Ray Skyvington in 1995, the Mississauga, Ont.-based SMI is a turnkey supplier of store fixtures and retail displays for customers across North America. For most of that time, the company focused on the design side of the business and outsourced the custom fabrication work. But eventually, to ensure timely delivery to customers, management decided to bring fabrication in-house.
“Initially, we worked as a sales and engineering service for our customers, but we kept running into supply chain issues,” said Brett Skyvington, manager of the company’s fabrication operations. “Six years ago, we took control of our metal fabrication needs by purchasing the equipment necessary to build what we considered our dream shop.”
“The companies we work with have very high quality control expectations, and the biggest thing that Brett picked up on when he set up the manufacturing operation was the quality that was required to be able to build and sustain a profitable company,” said Ray.
“We have clients that have been with us since we were founded in 1995. They are extremely loyal because of our attention to detail.”
Continuous Investments
Although its manufacturing operations have been up and running for only six years, SMI has continually invested in new equipment to ensure it can deliver what its customers require on time, to spec, and designed for comparatively easy and cost efficient manufacturing. The shop works in sheet, wire, and tube made of steel, stainless, aluminum, and other specialty metals. It also has moved into supplying glass, plastic, and wood fabrications, as well as peripherals like assembly, packaging, and graphics.
SMI currently runs an LVD 6-kW fiber laser equipped with a six-pallet tower and the company’s CADMAN programming software, a SafanDarley 100-ton electric press brake, and Baykal 160-ton and 60-ton hydraulic press brakes.
“The Safan is a relatively new purchase, with Wila premium tooling and hydraulic clamping,” Brett said. “We are also planning on investing in new software for the brakes so all of the programming can be programmed offline.
“We are primarily a small- to medium-run job shop,” Brett continued. “However, occasionally, jobs are much larger. We manufactured and distributed display cabinets to convenience stores and gas stations when a large vaping company came to Canada, which amounted to 30,000 cabinets in a year. We are equipped for those large runs. Today, you need that versatility to both prototype or run small jobs, as well as be able to scale up and run mass production.”
Welding Upgrades
“We are continuously assessing the tools and technology across the shop in order to upgrade as necessary,” Brett said. “Most recently, that has involved working through the welding department to see how we can become more efficient.”
The first investment, which occurred last November, was to replace all stations in the welding shop with Siegmund fixture tables.
“The simplicity that comes from not having to build jigs and fixtures is a huge time saver,” Ray said. “When you’re making a prototype for a client, that is very important. The first week we had the tables, we had to build three prototypes that would have taken the guys three to four days to make if they had to traditionally jig how they were going to put it together. With the efficiency gained by the fixture tables, we had all three prototypes made in less than a day.
“Previously, we would have tied up critical production of our top guys to building fixtures and lost floor space to fixture storage for those jobs,” he continued.
The newest purchase at the shop, however, is an ESAB cobot equipped with an Aristo 500ix power source and a Universal Robots robotic arm with a maximum reach of 51.2 in. Although it comes with a cart that allows it to be moved throughout a shop, SMI also attaches the arm to a 5- by 10-ft. table, allowing the operator to load parts on one side of the table while the cobot welds on the other side. Longer parts also can be affixed to be processed on the table.
“We previously had a traditional turntable-style welding cell,” Brett said. “It was difficult to program and not really suited to what we need on a day-to-day basis. We would run it a few times a year for very large-run production jobs that involved anywhere between 60 and 120 welds, but it would take forever to fixture and program. It didn’t suit our production mix and took up a lot of room.”
Cobot Choice
After talking with his team, Brett agreed that a cobot was a very good option. “It is really the way a lot of the industry is going, particularly for manufacturers of our size and weight class,” he noted.
Since installing the cobot in February 2023, SMI has already seen an impact.
“For example, we have been running a large fixture job, welding end caps and weld nuts onto thousands of tubes,” Brett said. “Each tube requires about 20 linear inches of welding, plus handling. We would have needed to bring on a second shift to run this program, but because of the versatility of the cobot, we can affix a number of these tubes to the side of the table as well as fixture them vertically and just run right through them. The cobot allows us to push quite a bit more volume through the shop without going out and having to staff additional shifts.”
At this time last year, SMI’s production ran 24 hours a day, six days a week. Now, it is running a shift and a half a day during the week and a single shift on Saturdays.
“And we are doing more volume at this point than we were doing last year,” Brett said. “Having the cobot and the tables has allowed us to specialize and to really focus on our core group of welders instead of scaling to handle production. Adding people for multiple shifts can lead to quality concerns; we want a core group of people who have a lot of industry experience or people with great attitudes who want to learn and who share our philosophy and attention to detail. These days, it’s crucial to understand what equipment is available to produce better and faster products because that is where the industry is heading.”
Dialed-In Precision
Like so many other shops, SMI is concerned about finding skilled employees. The company is fortunate to have very experienced employees heading up its forming, machining, and welding departments, but new technology will have to do the heavy lifting to keep production numbers high.
“Experienced welders and press brake operators are the hardest to find,” Brett said. “Finding press brake operators who understand integers, formulas, and bend radiuses are hard to find, and experienced welders in general are difficult to find. This is why we are investing in technology like the cobot and offline press brake programming software.”
In terms of improving weld throughput and quality, Brett noted, “How do you make a mediocre welder better? Give him better notches, better fit and finish in the parts that he is getting so then they’re not having to fill large gaps or get creative with their approach. Between our engineering department, the fiber laser, press brakes, and the fixturing tables, we are doing what we can to make that happen.”
In addition, being able to dial in the cobot to make more precise welds also saves time in postprocessing operations such as polishing.
Flexible Operations
The cobot is shipped on one skid and takes about two hours to put together, and it includes a cart. SMI often mounts the cobot on its 5- by 10-ft. table but likes having the ability to be able to move it to the cart in a matter of minutes for use elsewhere.
“We sometimes have three or four setups on the table that we run through at once,” Brett said. “At one point, we positioned it next to our spot welder. The operator spot welds the product where necessary, then turns around with the part, clamps it down, and the cobot MIG welds that part as the operator spot welds the next one. As long as it has an internet connection wherever it is placed, it can run without a problem.
“Using the fixturing tables, which are very precisely built, we can mount the cobot as required, repeatably to a very tight tolerance. There’s no need to touch up and check its alignment constantly, which was necessary with the robot on our old cell.”
SMI does its best to use the welding cobot where it can run three to four times faster than a person. Often, an operator will be doing whatever TIG work is necessary on an assembly while the cobot takes care of the MIG welds.
“It used to be that we needed large-run jobs to be able to utilize our robotic solutions, but now we can do it for much smaller runs. Being able to use an automated solution on jobs that were previously unfeasible for us is a big gain,” Brett said.
In terms of programming, Ray and Brett note that even nonwelders in the shop have learned to run the cobot.
“Using the app on your phone or tablet makes programming the cobot simple, and the app is very intuitive,” Brett said. “The guys got an hour training on it, watched a few videos, and we were programming jobs because it was so easy to use. It doesn’t involve a teach pendant, it doesn’t require you to program a lead-in to the weld. It’s very easy. In the same amount of time with a traditional robot, you’re still in the theory stage of how it is going to run.
“It’s also easy to make tweaks to the setups you’ve created. We do it all the time for different types of welds. For instance, you can globally change the wire feed speeds, heat, or voltage, depending on what you’re doing. With two clicks you can change the weld parameters across a whole program. It saves hours and hours of programming time.”
It’s also possible to monitor the welds throughout the day. The reporting software gives feedback on parts volume, wire feed speed, wire consumption, and gas consumption.
“We have full metrics on what parts are running, how many are running in a day, what programs have been run, and which operators were operating the cobot,” Brett said.
SMI ran thousands of components through the cobot in its first month of operation, amounting to 25,000 welds.
“In the first month, the ESAB cobot ran 2,600 of these different dividers that will go into a big box home improvement chain across the United Sates,” Brett said. “We then had it weld 600 tube caps and then a secondary process welding gussets for casters on 1,500 display bases. I think the cobot has averaged between 30 and 45 seconds a weld since it came into our shop. Over the course of the first month, the metrics available through the app confirmed we made 25,000 welds.”
Information Flow
This data is particularly important to SMI as it’s in the process of upgrading to the Epicor Kinetic ERP system. It will be integrating production data into the ERP system directly.
“We monitor as much as we possibly can in the company,” Brett said. “The new ERP system is going to make it easier to integrate all the data in the same place and better clarify our production flow and scheduling.”
SMI doesn’t have a huge footprint and works on a just-in-time (JIT) production model, which made Epicor’s JIT modeling capabilities a draw for them. Given that SMI can move from prototyping to full-scale production in a matter of hours is key.
“Ultimately, all of these investments are aimed at making a better, more affordable product for the customer,” Brett said.
“We encourage engineering and our designers to be able to work with production to say, ‘Hey look, how can we make a thing more effectively? What else can we modify and/or change to be able to improve the quality of the product and make it more repeatable in production?’” Ray said.
“Our goal is to pass the savings we are able to realize through good investments in technology and people back to our clients, while also being a lot more profitable ourselves. That has always been the directive right from the day Brett set the manufacturing operation up: We invest in good products that are going to be in the marketplace for a long time; we learn and teach our team better ways to do things and build that depth of knowledge so that the next time we're confronted with something, there are fewer questions that have to be asked between the front office and the shop to get to what we think is the right solution,” Ray continued.
“In the end, everyone benefits.”
About the Author
Robert Colman
FMA Communications Canada Inc. 1154 Warden Avenue Suite #416
Toronto, ON M1R 0A1 Canada
(815) 399-8700
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Why employee-owned companies make sense in manufacturing
What software automation means for custom fabrication
Nucor’s weekly steel price announcement continues to rattle markets
Press brakes, panel benders, and flat blank calculations
Washington artist creates life-size elk sculptures
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,