Miller Electric Mfg. Co. has increased the output of its Bobcat 250 and Trailblazer 302, Kohler gas-powered and Kubota diesel-powered welding machines/generators, to an Accu-rated 11,000 W of usable peak power. The machines can sustain the peak power for a minimum of 30 seconds at 104 degrees F, acc...
3/11/08
Hobart Brothers Co. offers low-alloy, gas-shielded, flux-cored wires suitable for high-pressure steam and gas piping, boiler manufacturing, and certain casting applications.
Designed for steels containing 1.25 percent chrome and 0.5 percent molybdenum, the TM-81B2 and TM-811B2 wires can be use...
7/10/07
Torch Wear® has introduced its X-Treme welding sleeve, featuring a three-layer design to provide protection.
Applications for the sleeve include carbon-arc, sub-arc, spray-arc, and heavy-arc welding, as well as pipe and heavy GTAW and standard GMAW. The sleeve exceeds Hazard Risk Category 4 s...
6/12/07
Arcos Industries LLC offers Arcos 1N12, a high-nickel covered electrode used to weld nickel-chromium-molybdenum alloys to themselves and to steel. It is also suitable for welding 5 and 9 percent nickel steels for low-temperature service to themselves, to low alloys, and to stainless steel.
The el...
6/12/07
Bore Repair Systems Inc.'s BOA-308i automatically replaces the worn-away steel in a bore using a simple GMAW process and common steel GMAW wire.
The positive-drive system is simple to operate, the company says.
2/13/07
UltraCore 712C and 712A80 gas shielded, flux-cored wires from The Lincoln Electric Co. are suitable for mild steel welding applications.
The 712C for tank and shipbuilding applications uses straight CO2. It is versatile and exhibits high impact values regardless of the notch location in the...
4/11/06
Select-Arc Inc. offers two low-alloy steel, gas-shielded, flux-cored electrodes with military specification approvals.
The Select 820-Ni1 produces 1 percent nickel weld deposit and welds steels that require low-temperature CVN toughness and moderate tensile strength (80,000 PSI). Specially formul...
2/7/06
The retrofit, 5 ¼- by 4 ½-in. variable-shade autodarkening replacement lens from Weldmark fits most 5- by 4-in. welding helmets.
The solar-powered lens includes a battery backup and has a 1.90- by 3.74-in. viewing area. Shade settings are 9 to 12, and the lens has adjustable sensitivity and delay...
12/13/05
Specialty Welds Ltd. offers a fully waterproof, autodarkening welding lens/filter for underwater wet welding.
The filter will fit into a standard Kirby Morgan welding assembly and provides a convenient welding or cutting accessory. Lifting the assembly up and down is unnecessary because the diver...
11/8/05
NovaTech's microscope-based welding systems let users see exactly where a weld puddle is applied for repairing tools and dies with minimal heat.
The microwelding systems produce a weld with less than 0.0005 in. of sink in the heat-affected zone (HAZ), which allows welds to last longer and reduces r...